3M SJ3571
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- Reclosable Loop Fastening
- Acrylic PSA Installation
- Configurable Roll Conversion
Product Description
3M Loop Fastener SJ3571 is an adhesive-backed woven nylon loop fastener for reclosable attachments used with a compatible 3M hook fastener. The soft napped loops engage the hook side for repeated opening and closing, while the acrylic pressure-sensitive adhesive mounts the loop to clean prepared surfaces without separate sewing or liquid adhesive. SJ3571 is commonly paired with 3M Hook Fastener SJ3572 and is available in multiple colors, widths, and roll lengths. Its preshrunk construction supports flat installation, and the adhesive is rated for long-term exposure to 93 deg C. The loop side is not a complete fastening system by itself.
Key features
- Reclosable loop function: Engages a compatible hook fastener for repeated access without screws, snaps, or zippers.
- Acrylic PSA attachment: Supports manual or automated mounting to clean, prepared surfaces.
- Configurable roll formats: Color, width, and roll-length options support conversion into application-specific pieces.
Applications
Applications include reclosable attachment of furniture cushions, signs, point-of-purchase displays, panels, and general industrial components.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Values are typical for the supplied loop fastener unless another status is shown.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Available colors | Beige, black, white | Current product options | |
| Loop material | Woven nylon | As supplied | |
| Adhesive | High-performance acrylic PSA | Pressure-sensitive backing | |
| Maximum unmated thickness | 3.2 | mm | Without liner; depends on compression |
| Liner thickness | 0.1 | mm | Polyolefin liner |
| Shelf life | 24 | months | Original packaging at 16 to 27 deg C and 40 to 60% RH |
After-processing / final-state properties
Mated performance requires a compatible hook fastener; peel and cycle values are typical under the stated conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Engaged thickness | 3.6 | mm | Mated fastener; depends on compression |
| 90 deg peel adhesion | 2.2 | lb/in width | 23 deg C; 304 mm/min; one fastener attached to non-anodized aluminum |
| Overlap shear strength | 22 | lb/in^2 | Nylon hook to nylon loop; 304 mm/min |
| Long-term temperature resistance | 93 | deg C | Exposure over days to weeks |
| Cycle life | 5,000 | closures | Nylon hook to nylon loop; number of closures before losing 50% of original peel strength |