LOCTITE ABLESTIK 8008HT

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik 8008HT

Main features

  • Thermally conductive
  • Low modulus
  • Stencil printing

Product Description

LOCTITE® ABLESTIK 8008HT adhesive is designed for high power devices in high UPH environment. It offers a lead-free alternative to soft solder and eutectic and can potentially reduce the layers of backside metallization required. This material can be applied to a wafer backside by stencil printing and then B-staged in an oven. The adhesive can then be cured after die attach in an in-line process exhibiting a consistent, void-free bondline without bleed.

LOCTITE ABLESTIK 8008HT should be used with a pressure sensitive dicing tape and is not compatible with UV dicing tapes. This hybrid chemistry product is thermally and electrically conductive and can be snap cured after B-stage.

 

Cure Schedule

  • 20 seconds @ 170°C. (Snap Cure)
  • 30 minutes ramp to 175°C + 60 minutes @ 175°C (Air box oven Cure)
Product Family

ABLESTIK 8008HT

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
264 °C
Thermal ConductivityThermal Conductivity
11 W/m.K
Chemical Properties
Moisture absorptionMoisture absorption
0.53 %
Physical Properties
Thixotropic indexThixotropic index
4.0
ViscosityViscosity
50,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers