LOCTITE ABLESTIK 965-1F
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Low modulus
- Low contaminants
- Low viscosity version of 965-1L
Product Description
LOCTITE ABLESTIK 965-1F electrically conductive die attach adhesive is designed for bonding large die to copper leadframes. It has stress absorbing properties and offers a low modulus of elasticity.
LOCTITE ABLESTIK 965-1F is a silver filled, higher viscosity version of ABLEBOND 965-1L adhesive.
Cure Schedule
- 1 hour @ 150°C
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Work life @25°CWork life @25°C
336 hoursChemical Properties
Water Extract pHWater Extract pH
4.6Physical Properties
ViscosityViscosity
18,000 mPa.s