LOCTITE ABLESTIK ATB 120U

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

LOCTITE ABLESTIK ATB 120ULOCTITE ABLESTIK ATB 120U

Main features

  • Non conductive
  • Thin bondline
  • Fast cure

Product Description

LOCTITE® ABLESTIK ATB 120U Non conductive adhesive film is formulated for use in wafer lamination and chip on chip processes. It combines process ease with the proven reliability of Henkel materials. It is the most transparent film available for high volume applications and is widely used for glass attach in smart phones (bonding the finger print sensor “under glass”).This 2 in 1 format is designed for base die and die to die (>1x1mm) applications, moving to thing wafer (<100um). It is a product with good workability, excellent flow ability on the substrate and a good candidate when using a Si spacer die for CoC processes.

LOCTITE® ABLESTIK ATB 120U Non conductive adhesive film has a thickness of 20um but is also available in 10, 30 and 40um. It can be used to absorb CTE mismatch between substrates but the extend to which it can be effective will depend on the bond area. The bigger the parts, the bigger the mismatch and stress. Even flexible adhesives won’t behave that flexible when thin bond lines need to absorb stress in larger bond areas. For example the glass wind shield in cars is bonded with flexible PUR adhesive with ±2-3mm bond line thickness to absorb movements. So from a Die attach film perspective, a 20um bond line will give half the stress compared to 10um!

LOCTITE® ABLESTIK ATB 120U is a medium modulus die attach film on dicing tape with 20um transparent thermoset epoxy layer that is DBG (Dicing before grinding) compatible. This means that (contrary to the "normal" process) the wafer is half cutted and the die separation happens during the backside grinding process.

Cure Schedule

  • 30 minute ramp to 120°C + 30 minutes @ 120°C
Product Family

ABLESTIK ATB120U

1. Select Package Type
2. Select Pieces per roll
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 48 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Please select Package Type and Pieces per roll.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive ThicknessAdhesive Thickness
20 µm
Film ThicknessFilm Thickness
85 µm
Total ThicknessTotal Thickness
105 μm
Work life @25°CWork life @25°C
720 hours
Thermal Properties
Thermal ConductivityThermal Conductivity
0.21 W/m.K

Additional Information

Figure. ATB 120U Transmittance vs Other films light transmittance

How do you use Die attach films?

These dicing die attach adhesive films are supplied on a wafer dicing tape, being laminated on a wafer which can be diced and then a typically dry to touch “B-staged” adhesive of 10-40um will be left of the die back (of part) before final bonding step. Todays’ thinnest version is ATB 110U with 10um adhesive layer after removing the release liner and dicing tape. Note that surface roughness and warpage needs to be compensated to prevent voids during and after cure, so 20um is more commonly used.

What Dk/Df data do we have for these materials?
We do not have dk/df for these specific thicknesses but please see data at much lower frequencies on hand attached for reference. Looking at the down trend at higher frequencies and other epoxy based materials tested, we estimate Dk ~3 for these film materials at 28 GHz ...

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers