ALPHA SACX Plus 0307

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

ALPHA SACX Plus 0307

Main features

  • Low dross formation
  • Excellent mechanical reliability
  • Made with Vaculoy technology

Product Description

ALPHA SACX Plus 0307 is a next generation lead-free alloy suitable for use as a replacement for SnPb, SAC305 and other low silver SAC alloys including the original SACX 0307 in wave solder, lead tinning and rework processes. SACX Plus 0307 has been engineered for improved copper dissolution performance during the long hot exposure times associated with rework and lead tinning. The SACX Plus 0300 variant is used as a replenishment alloy in solder baths with elevated copper levels. As with all Alpha Metals bar solder, Alpha’s proprietary Vaculoy®manufacturing process is used to remove certain impurities, particularly oxides. The product is further enhanced with the addition of other materials designed to further reduce drossing, increase wetting speed and force and improve joint cosmetics.

Product Key Features

  • Manufactured using Alpha’s proprietary Vaculoy® process to remove impurities and oxides
  • Enhanced copper control
  • Reduced dross formation
  • Superior wetting performance

Applications

  • Ideal for wave solder, lead tinning and rework processes.
Product Family

ALPHA SACX PLUS 0307

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Coefficient of Thermal Expansion (CTE), α1Coefficient of Thermal Expansion (CTE), α1
1.79e-5 ppm/°C
Coefficient of Thermal Expansion (CTE), α2Coefficient of Thermal Expansion (CTE), α2
2.3e-5 ppm/°C
Liquidus Melting TemperatureLiquidus Melting Temperature
228 °C
Solidus Melting TemperatureSolidus Melting Temperature
217 °C
Specific Heat CapacitySpecific Heat Capacity
0.00017 J/(g⋅°C)
General Properties
DensityDensity
7.33 kg/m3
Mechanical Properties
ElongationElongation
21.8 %

Additional Information

Application Guidelines

ALPHA SACX Plus 0307 is suitable for wave soldering, lead tinning and reworking through hole and surface mount components in a lead-free process. It is suited to single side and relatively complex, dual sided mixed technology boards. A solder pot temperature of 255 to 265 °C (491 to 509 °F) is recommended with a contact time 2.3 to 3.5 seconds. For suitable wave solder fluxes, contact your local sales representative. Lead free Reclaim services including dedicated lead free containers is also available, consult your local Alpha sales office.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF