BONDERITE M-CR 1132 AERO TOUCH-N-PREP PEN

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE M-CR 1132 AERO TOUCH-N-PREP PEN

Main features

  • Ready-to-Use Touch-N-Prep Pen
  • No-Rinse Dry-in-Place Processing
  • Modifiable Felt-Tip Applicator

Product Description

BONDERITE® M-CR 1132 AERO Touch-N-Prep® Pen is a ready-to-use hexavalent chromium conversion coating applicator for localized touch-up and repair of aluminum and aluminum-alloy surfaces. The dry-in-place treatment is applied directly from the pen without rinsing and may be air-dried or force-dried with warm air. Its controlled felt-tip delivery system supports treatment of edges, holes, rivets, and other small or difficult-to-reach areas while reducing chemical use, worker contact with chromating solutions, and rinse-water waste compared with conventional chromating processes.

Key Features

  • Ready-to-use conversion coating: Delivers a dry-in-place hexavalent chromium treatment directly from the applicator pen without mixing or dilution.
  • No-rinse application: The applied coating can be air-dried or force-dried with warm air at a maximum recommended temperature of 60°C (140°F).
  • Controlled touch-up delivery: The felt-tip applicator supports localized treatment of edges, holes, rivets, and other small or difficult-to-reach aluminum surfaces.

Applications / Suitable for

  • Touch-up and repair of conversion coatings on aluminum and aluminum-alloy surfaces
  • Localized treatment of bare areas on aircraft and aircraft-part surfaces
  • Treatment of edges, rivets, holes, and other small or difficult-to-reach areas
Product Family

BONDERITE M-CR 1132

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Felt-tipped type marker / Colorless

Additional Information

Technical Properties

After-Processing / Final-State Properties

Typical coating-weight and coverage guidance when two coats are applied.

Property Value Unit Method / Condition
Light Coating Weight 13 to 18 mg/ft² Class 1A and Class 3; two coats; approximately 50 ft² coverage per pen
Moderate Coating Weight 18 to 22 mg/ft² Class 1A and Class 3; two coats; approximately 35 ft² coverage per pen
Heavy Coating Weight 22 to 35 mg/ft² Class 1A only; two coats; approximately 25 ft² coverage per pen
Minimum Double-Coat Weight At least 10 mg/ft² When the applicator pen adequately wets the surface

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers