BONDERITE M-CR 1200S
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- MIL-DTL-5541 Qualified Aluminum Coating
- Immersion, Spray, or Brush Application Flexibility
- Wide-Range Bath Operating Window
Product Description
BONDERITE M-CR 1200S AERO is a brown powdered chromate conversion-coating chemical used to treat aluminum and its alloys. Mixed into an aqueous bath and applied by immersion, spray, or brush, it forms a light iridescent golden-to-tan coating that reduces corrosion and improves paint adhesion. The bath operates at a pH of 1.3 to 2.1 and a temperature of 20 to 35 deg C (68 to 95 deg F), with a contact time of 15 seconds to 3 minutes. Immersion or spray baths are built up at 6.3 lb per 100 gallons, while brush-application baths use 12.5 lb per 100 gallons. The coating chemical is listed on Qualified Product List QPL-81706 as an approved material for Class 1A and Class 3 coatings, bare or painted, in accordance with MIL-DTL-5541.
Key features
- Immersion, Spray, or Brush Application: applied to aluminum by immersion, spray, or brush depending on process needs
- MIL-DTL-5541 Qualified Coating: listed on QPL-81706 as an approved material for Class 1A and Class 3 coatings
- Wide Operating pH and Temperature Range: bath operates at pH 1.3 to 2.1 and 20 to 35 deg C (68 to 95 deg F)
Applications
Chromate conversion coating of aluminum before painting or for corrosion-protection processes.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Brown powder | - | As supplied |
| Bath pH | 1.3 to 2.1 | pH | Operation and control; optimum 1.3 to 1.8 |
| Operating temperature | 20 to 35 (68 to 95) | deg C (deg F) | Immersion, spray, or brush bath |
| Contact time | 15 to 180 | sec | Immersion, spray, or brush application |
| Bath makeup, immersion or spray | 6.3 | lb per 100 gal | Chemical / bath preparation |
| Bath makeup, brush | 12.5 | lb per 100 gal | Chemical / bath preparation |