BONDERITE S-FN 310A

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE S-FN 310A

Main features

  • PTFE Dry-Film Low-Friction Release
  • Longer Wear Life than Pure PTFE
  • 149 deg C Low-Temperature Cure

Product Description

BONDERITE S-FN 310 ACHESON (formerly EMRALON 310) is a two-component, phenolic resin-bonded PTFE dry film coating and lubricant. It cures at a low temperature of 300°F (149°C) and is designed to provide excellent surface adhesion, a low coefficient of friction, corrosion resistance, and good release properties on materials such as wood, metal, rubber, and plastics.

Key features

  • Superior wear life: Delivers a longer wear life and more uniform thickness than pure PTFE coatings.
  • Low friction and release: Provides an as-applied static friction coefficient between 0.05 and 0.07, along with excellent release properties.
  • Low temperature cure: Enables application on substrates where conventional PTFE coatings cannot be used by curing at 300°F (149°C).

Applications / Suitable for

  • Lubrication and release coating on wood, metal, rubber, and plastics.
  • Applications requiring a low coefficient of friction.
  • Substrates that require a low-temperature curing PTFE coating.
Product Family

BONDERITE S-FN 310A

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Phenolic resin-bonded PTFE dry film coating and lubricant
Thermal Properties
Operating TemperatureOperating Temperature
177°C (350°F) continuous service / 204°C (400°F) intermittent service °C

Additional Information

Technical properties

As-supplied / before-processing properties

Physical and processing characteristics of mixed BONDERITE S-FN 310 ACHESON.

Property Value Unit Method / condition
Mix Ratio (Weight) 22:100 - Part A (White) to Part B (Blue)
Consistency Liquid - -
Density (As Applied) 8.2 lb/gal -
Flash Point 46 (9) °F (°C) -
Pot Life 24 hours -
Application Method Spray - Cannot be dipped or brushed
Technical properties

After-processing / final-state properties

Typical cured film properties of BONDERITE S-FN 310 ACHESON.

Property Value Unit Method / condition
Color (Cured) Light green - Typical
Friction Coefficient (Static) 0.05 to 0.07 - As applied
Service Temperature 350 (177) °F (°C) -
Intermittent Temperature 400 (204) °F (°C) Avoid temperatures in excess of this

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers