DOWSIL 3-6891

Main features

  • Machinable Abradable Rubber
  • 0.95 Cured Specific Gravity
  • Two-Hour 300 deg F Cure

Product Description

DOWSIL 3-6891 Abradable Sealant starts as a black, flowable one-part silicone and heat-cures into a low-density, flexible and machinable rubber. A Brookfield viscosity of 2,300 poise supports casting, troweling or injection with standard one-component equipment, while a two-hour cure at 300 deg F establishes the condition for the cured-property values. The cured material combines a specific gravity of 0.95, Shore A 71 hardness, 580 psi tensile strength and 0.24 W/(m K) thermal conductivity. Applications include abradable seals, compressor-blade rubstrips and high-temperature thermal insulation.

Key features

  • Abradable cured rubber: The heat-cured material can be machined for controlled seal clearance.
  • Low-density final state: Typical cured specific gravity is 0.95.
  • Heat-cure processing: Cured-property values use a two-hour cure at 300 deg F.

Applications

Abradable seals, compressor-blade rubstrips and high-temperature thermal-insulation applications.

Product Family

DOWSIL 3-6891

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Black, flowable liquid
Specific GravitySpecific Gravity
0.95
Physical Properties
ViscosityViscosity
230,000 mPa.s
Mechanical Properties
ElongationElongation
70 %
Thermal Properties
Thermal ConductivityThermal Conductivity
0.24 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and storage properties. Values are not specifications.

Property Value Unit Method / condition
Physical form Flowable liquid As supplied
Appearance Black As supplied
Viscosity 2300 poise Brookfield HAF #7 at 10 rpm
Shelf life 12 months Original unopened container
Storage temperature 15-40 deg F Original unopened container
Package size 3.6 kg Pail
Technical properties

After-processing / final-state properties

Typical properties after a two-hour cure at 300 deg F.

Property Value Unit Method / condition
Physical form Flexible rubber After heat cure
Specific gravity 0.95 After heat cure
Durometer hardness 71 Shore A After heat cure
Tensile strength 580 psi After heat cure
Elongation 70 % After heat cure
Lap shear adhesion 320 psi Aluminum; 100% cohesive failure
Thermal conductivity 0.24 W/(m K) After heat cure
Coefficient of thermal expansion 1.75 x 10^-4 m/m deg C After heat cure

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers