LOCTITE ECCOBOND D125 F DR
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Main features
- Low water absorption
- Low exotherm
- Non-sag
Product Description
LOCTITE D 125 F DR is a epoxy surface-mount adhesive designed for high-speed dispensing.
LOCTITE D 125 F DR is used in a wide array of applications, including chip capacitors, chip resistors, SOTs, SOICs, and PLCCs.
Technical Specifications
General Properties
Specific GravitySpecific Gravity
1.275Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
85 °CThermal ConductivityThermal Conductivity
0.3 W/m.KElectrical Properties
Volume ResistivityVolume Resistivity
1000000000000000 Ohms⋅cmAdditional Information
TYPICAL CURING PERFORMANCE
IR or Convection Conveyor Oven
20 minutes @ 100°C
7 minutes @ 110°C
2.5 minutes @ 120°C
1.5 minutes @ 150°C
Convection Box Oven
30 minutes @ 100°C
20 minutes @ 110°C
10 minutes @ 120°C
5 minutes @ 150°C