LOCTITE ECCOBOND F113SC

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND F113SC

Main features

  • Two component
  • High Tg
  • Fiber optic assembly

Product Description

LOCTITE ECCOBOND F113SC is a two-component epoxy that is formulated for terminating all types of fiber optic connectors. This high Tg and low viscosity product is used to create low stress connections with no pistoning. Its dark blue color (after mixing) allows for easy polishing

LOCTITE ECCOBOND F113SC can operate in temperatures between -60 to 120°C and is typically used for Fiber optic connectors, LED displays, Lenses and Optoelectronic device assembly.

 

Cure Schedule

  • 18 hours @ 25°C or
  • 1 hour @ 65°C or
  • 15 minutes @ 90°C (for one drop applications)
Product Family

ECCOBOND F113SC

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 30 days
CA Shipping in 12 weeks
EU Shipping in 55 days
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot LifePot Life
0.5 hours
Refractive indexRefractive index
1.52
Specific GravitySpecific Gravity
1.1
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
95 °C
Chemical Properties
Water AbsorptionWater Absorption
0.98 %
Physical Properties
ViscosityViscosity
1800 mPa.s

Additional Information

How to use

  1. Carefully clean and dry all surfaces to be bonded
  2. Remove clamp and thoroughly mix the LOCTITE ECCOBOND F113SC epoxy adhesive system components in the handy BIPAX mixing-dispenser package until color is uniform throughout
  3. Apply this completely mixed adhesive to the prepared surfaces, and gently press these surfaces together. Contact pressure is adequate for strong, reliable bonds; however, maintain contact until adhesive is completely cured
  4. Some separation of components is common during shipping and storage. For this reason, it is recommended that the contents of the shipping container be thoroughly mixed prior to use
  5. Some ingredients in this formulation provided in BIPAX, TRA-PAX and bulk packaging may crystallize when subjected to low temperature storage. A gentle warming cycle of 52ºC for 30 minutes prior to mixing components may be necessary. Crystallized epoxy components do not react as well as liquid components and should be redissolved prior to use for best results

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers