ELANTAS CE-1164

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ELANTAS CE-1164

Main features

  • Transparent Conformal Coating
  • 20 to 30-Minute Tack-Free Time
  • 500 V/mil Dielectric Strength

Product Description

CONATHANE® CE-1164 Polyurethane Conformal Coating is a solvent-borne, single-component, transparent polyurethane conformal coating for thin-film protection of printed circuit boards and electronic components. The fast-curing coating may be sprayed, dipped, or brushed and includes fluorescence for inspection under ultraviolet light. It is documented for electrical and moisture-barrier performance, hydrolytic stability, flexibility, and adhesion to phenolic and epoxy-glass laminates. Typical as-supplied properties include 100 cP viscosity and 50% solids, with tack-free time of 20 to 30 minutes and full cure in 24 hours at 25°C.

Key features

  • Fast-curing polyurethane coating: Typical tack-free time is 20 to 30 minutes with 24-hour cure at 25°C.
  • UV inspection aid: The transparent coating fluoresces under ultraviolet light.
  • Electrical insulation: Typical cured data include 3,500 V/mil dielectric strength and 1.5 × 10¹⁵ ohm·cm volume resistivity.

Applications / Suitable for

  • Thin-film coating of printed circuit boards
  • Electrical and moisture protection of components
  • Phenolic and epoxy-glass laminate assemblies
Product Family

ELANTAS CE-1164

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or processing-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Product form Single-component solvent-borne coating N/A As supplied
Appearance Clear light amber N/A As supplied
Viscosity 100 cP At 25°C
Specific gravity 1.05 N/A At 25°C
Solids content 50 % 135°C for 45 min
Flash point 7 °C ASTM D93
Tack-free time 20 to 30 min At 25°C
Full cure 24 h At 25°C
Technical properties

After-processing / final-state properties

Typical cured or final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Dielectric strength 3,500 V/mil ASTM D149 at 25°C
Volume resistivity 1.5 × 10¹⁵ ohm·cm ASTM D257 at 25°C
Dielectric constant 2.7 N/A ASTM D150 at 1 MHz and 25°C
Dissipation factor 0.02 N/A ASTM D150 at 1 MHz and 25°C
Thermal shock Pass N/A MIL-STD-810B, -65°C to 125°C
Hydrolytic stability No discoloration or degradation N/A 120 days at 85°C and 95% RH

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers