EPOCAP 47577

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

EPOCAP 47577

Main features

  • UL 94 V-0 Classification
  • Non-Abrasive Filler for Automated Dispensing
  • 206-Minute Working Window

Product Description

EPOCAP® 47577/57577 (formerly EPOCAP® 17577) is a two-component, room temperature curing epoxy encapsulation system specifically designed for protecting submersible pump equipment. It features excellent cured properties and is formulated with non-abrasive inert fillers, making it well-suited for processing through automated dispensing equipment.

Key features

  • Flame retardant: Recognized to meet UL 94 V-0 flame retardancy standards at a thickness of 0.250".
  • Machine-friendly formulation: Contains non-abrasive inert fillers that minimize wear and facilitate ease of use in automated dispensing equipment.
  • Extended working time: Provides a long pot life with a gel time of 206 minutes for a 100-gram mass at 25°C, accommodating large or complex potting applications.

Applications / Suitable for

  • Encapsulation of submersible pump equipment.
  • General potting applications requiring UL 94 V-0 flame retardancy.
  • High-volume automated dispensing processes.
Product Family

EPOCAP 47577

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Black
Specific GravitySpecific Gravity
1.52 g/cm³
Physical Properties
ViscosityViscosity
3,500 (Mixed) mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure processing characteristics of mixed EPOCAP® 47577/57577.

Property Value Unit Method / condition
Appearance / Color (Mixed) Black - -
Mix Ratio (Weight) 100:13 - Part 47577 to Part 57577
Mix Ratio (Volume) 100:22 - Part 47577 to Part 57577
Viscosity (Mixed) 3,500 cps at 25°C
Specific Gravity (Mixed) 1.52 - at 25°C
Gel Time (100 gm mass) 206 minutes at 25°C
Gel Time (10 gm mass) 40 minutes at 60°C
Technical properties

After-processing / final-state properties

Typical cured mechanical, thermal, and electrical properties of EPOCAP® 47577/57577.

Property Value Unit Method / condition
Hardness 88 Shore D Tested at 25°C
Tensile Strength 6,150 psi Tested at 25°C
Compressive Strength 12,700 psi Tested at 25°C
Flexural Strength 10,700 psi Tested at 25°C
Linear Shrinkage 0.0011 in./in. Tested at 25°C
Heat Distortion Temperature 48 °C -
Recommended Service Temperature 105 °C -
UL Flame Retardancy Pass - UL 94 V-0 @ 0.250"
Dielectric Strength 378 volts/mil -

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers