HumiSeal Stripper 1063
Harmonization Code : 3814001000 |

Main features
- Non-Acidic Polyurethane Removal
- Controlled One-Hour Soak
- Clear Low-Density Stripper
Product Description
HumiSeal Stripper 1063 is a non-acidic liquid stripper for dissolving cured HumiSeal polyurethane conformal coatings from printed wiring board assemblies. The clear product has a specific gravity of 0.84 +/- 0.01, a relative evaporation rate of 2.10, and a TCC flash point of 11.1 deg C. The stated removal process uses a 60 minute immersion, brushing of loosened material, final cleaning with isopropyl alcohol and deionized water or another qualified cleaner, inspection, and a 30 minute bake at 60 to 65 deg C after final cleaning.
Key features
- Non-acidic polyurethane coating removal: The stripper is formulated to dissolve cured HumiSeal polyurethane conformal coatings.
- Controlled 60-minute immersion: The documented process uses a one-hour soak before brushing and final cleaning.
- Clear low-density liquid: The product is supplied as a clear liquid with a specific gravity of 0.84 +/- 0.01.
Applications
- Removal of cured HumiSeal polyurethane coatings from printed wiring board assemblies
TDS, SDS & Technical Documents
Technical Specifications
General Properties
ColorColor
ClearEvaporation RateEvaporation Rate
2.1Specific GravitySpecific Gravity
0.82Thermal Properties
Flash PointFlash Point
11.1 °CAdditional Information
Technical properties
As-supplied / before-processing properties
Typical liquid properties and shelf life before the coating-removal process.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Clear liquid | - | As supplied |
| Relative evaporation rate | 2.10 | - | Typical liquid value |
| Specific gravity | 0.84 +/- 0.01 | - | Typical liquid value |
| Flash point | 11.1 | deg C | TCC |
| Shelf life | 12 | months | As supplied in the original container |