HumiSeal Thinner 904

Harmonization Code : 3814001000 |

HumiSeal Thinner 904

Main features

  • Faster evaporation rate
  • Smoother flow
  • Faster drying time

Product Description

Consider using HumiSeal Thinner 904 when smooth flow, leveling, and controlled drying on 1B51NS/NSLU coatings are required.

Product Key Features

  • Slightly faster evaporation rate than Thinner 903
  • Excellent for applications requiring faster drying

Applications

 

Product Family

HUMISEAL 904

1. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 6 weeks
TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Clear
Specific GravitySpecific Gravity
0.77
Vapor DensityVapor Density
4.0
Vapor PressureVapor Pressure
2.8 mmHg
Thermal Properties
Boiling PointBoiling Point
110 °C
Flash PointFlash Point
-6 °C

Additional Information

Directions for Use

  • Add HumiSeal® Thinner to a compatible coating until the desired viscosity is obtained.

Handling Precautions

HumiSeal® Thinners are flammable and the following standard safety precautions should be observed:   

  • Use only in well ventilated areas.   
  • Protective gloves and goggles should be worn.   
  • In case of prolonged skin contact, wash with water.   
  • In case of eye contact, flush with water and contact physician.   
  • Avoid prolonged breathing of vapors.  
  • Unused portions of HumiSeal® products must be disposed of in strict compliance with Local, State, and Federal laws governing such matters.   
  • Consult the Material Safety Data Sheet (MSDS/SDS) for more specific product information. 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers