Hysol GR2220 | Black Epoxy Mold Compound
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other



Main features
- Designed for MnO-based tantalum capacitors
- Lower cost of ownership
- High productivity, easily moldable
Product Description
Hysol GR2220 black epoxy molding compound delivers outstanding performance and ease of use. It is a "Green" environmentally friendly product with 75% fused silica filler that has high moldability and fast cycle time.
Hysol GR2220 is a heat curable epoxy, mainly used for MnO tantalum capacitors and can reach a VO flammability rating. It has been formulated to provide the best possible moldability and as wide molding latitude as possible.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
ColorColor
BlackFiller ContentFiller Content
75 %Specific GravitySpecific Gravity
1.82Physical Properties
Spiral Flow @ 175°CSpiral Flow @ 175°C
81.28 cmThermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
161 °CUL 94 RatingUL 94 Rating
V0Curing Conditions
Transfer PressureTransfer Pressure
40 - 80 kg/cm2Transfer TimeTransfer Time
5 - 15 s