TMC-8020LS | Clear Optical Molding Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

TMC-8020LS | Clear Optical Molding Compound

Main features

  • LED Encapsulation
  • Low stress
  • Better reflow and Thermal shock

Product Description

OPTOLINQ TMC-8020-LS is a high-performance optical solid epoxy specifically developed for LED encapsulation. This monocomponent epoxy achieves superior adhesion performance and great transmittance. It has lower Tg than the "normal" 8020 version.

OPTOLINQ TMC-8020-LS is able to offer low blue-ray decay for outdoor LED applications and overall great light performance. This low stress white epoxy is very close to competitive solutions such as XX814, XX1000 and XX97. It is a reliable product that has improved reflow abilities and thermal shock test performance.

Product Family

LINQ TMC-8020LS

1. Select Package Type
2. Select Pellet Size
3. Select Pellet Weight
4. Select Transmittance
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks

Technical Specifications

General Properties
AppearanceAppearance
Blue Tablet
Specific GravitySpecific Gravity
1.2
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
95 °C
Chemical Properties
Water AbsorptionWater Absorption
0.17 %
Curing Conditions
Transfer PressureTransfer Pressure
10 - 40 kg/cm2
Transfer TimeTransfer Time
20 - 50 s
Physical Properties
Spiral Flow @ 175°CSpiral Flow @ 175°C
150 - 250 cm

Additional Information

 
 TMC-8020 Low Stress Products Properties Comparison
 
PROPERTY UNIT TMC-8020L TMC-8020LS
Viscosity  cP 300 200
Spiral Flow @150°C cm 150-250 150-250
Hot Plate Gel Time @150°C sec 25-50 20-50
Glass Transition Temperature °C 115 95

CTE by TMA, α1

CTE by TMA, α2

ppm

ppm

70

170

70

220

Moisture Absorption PCT

24 hrs @25°C water

24 hrs @121°C, 2atm, 100%RH

 

wt%

wt%

 

0.16

3.2

 

0.17

3.8

Flexural Strength @25°C

Flexural Modulus @25°C

MPa

Mpa

130

2900

110

3100

yellowing Δb - 4 hrs @200°C

yellowing Δb - 30 min @280°C

yellowing Δb - 4 hrs UV

-

8

42

16.5

25

45

16.5

Transmittance 1mm @450nm % >90 >90
Refractive Index @633nm - 1.56 1.56
Comment   Low stress version for better reflow performance Low stress for balanced reflow and thermal shock test performance
 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers