TMC-9000T | Clear Optical Molding Compound
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Main features
- Transparent Filler Technology
- Anti-blue Decay
- Low CTE & Low Moisture Absorption
Product Description
OPTOLINQ TMC-9000T is a high-performance optical solid epoxy specifically developed for white decorative and backlight LED encapsulation. This monocomponent epoxy achieves superior adhesion performance and great transmittance. Its stability at high temperature aids towards a good package performance and long life. More important, TMC-9000T applies transparent filler technology to achieve low CTE and low moisture absoprtion.
TMC-9000T is developed based on TMC-8060 formula, which is able to offer low blue-ray decay for outdoor LED applications and overall great light performance. This anti yellowing white epoxy is very close to competitive solutions such as XX814, XX1000 and XX97.
Reliability Tests Passed:
- Thermal cycling, -45°C ~ 100°C * 500 cycles
- Double 85, 85°C * 85%RH * 168hrs
- High temperature storage, 150°C * 1000hrs
- Reflow, 260°C * 10s * 3 times
Other Versions In TC-8060 Series:
- TMC-8060 Orignal Version
- TMC-8060-IMP Low modulus version
To Know More about TC-9000T:
- TMC-8060 Series Anti-blue Decay Data
- TMC-9000T High Temperature Storage Data
- TMC-9000T Filler Content Data
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Curing Conditions
Physical Properties
Additional Information
To meet higher MSL test requirements, clear molding compound is expected to have (1) low moisture absorption; (2) low stress generated; (3) low CTE. Our filler technology could helpmeet these challenges. With the content of filler increasing in TMC-9000T, the CTE and water absorption both decrease. Meanwhile, TMC-9000T is based on the TMC-8060 product platform, TMC-9000T remains the superior anti-blue decay property as TMC-8060. Worth to be mention, the straight light R-transmittance will also decrease a lot with filler content increase. Thus, we usually keep the filler content in the range of 40~80% based on specific application needs.