LOCTITE AA 3526
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- Translucent
- Cures rapidly
- Excellent adhesion to glass, plastics and metals
Product Description
LOCTITE® AA 3526 is a translucent, pale straw to amber, 1-part, medium viscosity, UV/visible light-cured, liquid modified acrylic adhesive. It cures rapidly to form flexible, transparent bonds when exposed to ultraviolet light and/or visible light of sufficient irradiance. The secondary cure system permits cure of product in shadowed areas.
LOCTITE® AA 3526 is an Acrylic, monocomponent liquid with positive fluoresence under UV light. It's bonding cure profile benefits high speed curing production lines.
LOCTITE® AA 3526 can be cured by exposure to UV and/or visible light radiation or heat . The speed and depth of cure will depend on the UV intensity measured at the product surface.
Heat Cure
- 15minutes at 121°C
Fixture Time
Fixture time is defined as the time to develop a shear strength of 0.1 N/mm².
UV Fixture Time, Glass microscope slides, seconds:
- Black light, Zeta® 7500 light source:
- 6 mW/cm², measured @ 365 nm ≤5LMS