LOCTITE E-40FL
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Toughened Epoxy Bonding
- Medium Owrking Life
- Shock and Vibration Resistance
Product Description
LOCTITE® EA E-40FL™ is a toughened, medium-viscosity, two-component epoxy adhesive designed for flexible bonding applications requiring excellent shock and impact resistance. After mixing, the adhesive cures at room temperature to form a flexible gray bond line with strong adhesion to plastics, metals, glass, wood, ceramics, rubber and masonry. The cured material provides good chemical and solvent resistance together with excellent electrical insulation characteristics, making it suitable for bonding dissimilar materials and low-stress, high-impact assemblies.
Key Features & Benefits
- Toughened two-component epoxy adhesive.
- Flexible cured bond line with excellent impact resistance.
- Medium working life for convenient assembly operations.
- Excellent resistance to shock and vibration.
- Good chemical and solvent resistance after cure.
- Excellent electrical insulation properties.
- Suitable for bonding dissimilar materials.
Recommended Applications
- Plastic, metal, glass and ceramic bonding.
- Rubber-to-metal bonding applications.
- Repair of strain gauges and printed circuit boards.
- Sealing fiberglass component seams.
- Bonding stainless steel inserts and hose assemblies.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Condition |
|---|---|---|---|
| Technology | Epoxy | — | Two-component adhesive |
| Appearance (Resin) | Off-white to Beige Liquid | — | Part A |
| Appearance (Hardener) | Dark Gray Liquid | — | Part B |
| Appearance (Mixed) | Gray Opaque Liquid | — | Mixed adhesive |
| Mix Ratio (Volume) | 1 : 1 | Resin : Hardener | By volume |
| Mix Ratio (Weight) | 100 : 85 | Resin : Hardener | By weight |
| Resin Viscosity | 60,000 - 90,000 | mPa·s (cP) | Brookfield RVT, 25°C |
| Hardener Viscosity | 50,000 - 85,000 | mPa·s (cP) | Brookfield RVT, 25°C |
| Specific Gravity (Mixed) | 1.2 | — | 25°C |
| Working Life | 40 | minutes | 25°C |
| Tack Free Time | 130 | minutes | Typical |
After-Processing / Final-State Properties
| Property | Value | Unit | Condition / Method |
|---|---|---|---|
| Glass Transition Temperature (Tg) | 30 | °C | Cured @ 25°C |
| Shore Hardness | 75 | Shore D | ISO 868 |
| Elongation | 22 | % | ISO 527-2 |
| Tensile Strength | 16 | N/mm² | ISO 527-2 |
| Dielectric Breakdown Strength | 16 | kV/mm | IEC 60243-1 |
| Lap Shear Strength (Aluminum) | 25.9 | N/mm² | 3 days @ 22°C |
| Lap Shear Strength (Steel) | 4.4 | N/mm² | Grit blasted steel |
| Block Shear Strength (Epoxy) | 11 | N/mm² | ISO 13445 |
| Block Shear Strength (Glass) | 12.9 | N/mm² | ISO 13445 |