LOCTITE EDAG PF 410 E&C

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE EDAG PF 410 E&C

Main features

  • Screen printable
  • Excellent print definition
  • Silver filled

Product Description

LOCTITE EDAG PF 410 E&C is designed for production of flexible circuitry. This material can be used on a variety of substrates and is applicable with manual, semi automatic or high speed reel to reel screen printing equipment.

LOCTITE EDAG PF 410 E&C is passed over a triple roll mill to remove small particles. It offers extended screen residence time and excellent print definition with superior adhesion to polyester film.

Drying Cycle

  • 30 minutes @ 80°C or
  • 15 minutes @ 120°C

LOCTITE EDAG PF 410 E&C can be dried immediately after printing at temperatures between 80 to 140°C

Product Family

LOCTITE EDAG PF410

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 93 days
CA Shipping in 12 weeks
EU Shipping in 25 days
TDS, SDS & Technical Documents

Technical Specifications

General Properties
SolidsSolids
75 %
Physical Properties
ViscosityViscosity
17,500 mPa.s

Additional Information

Optimal Storage : 5 to 30 °C

TYPICAL SCREEN PRINTING PROCESS
Recommended Thickness
-Applied dry coating thickness , μm 8 to 12


Emulsion Thickness
-Emulsion Thickness , μm 20 to 40

Recommended Squeegee
-Polyurethane , durometer 70 to 75

Recommended Screen Type
-Monofilament polyester screen, threads/cm 68 to 110
-Stainless steel screen , threads/cm 90 to 154

Printing Equipment Type
-Manual
-Semi-automatic
-High speed reel-to-reel

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers