LOCTITE LB8009
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

Main features
- Steel Compatibility Paste Material
- Improved Clamp Load Consistency
- Non-Curing Assembly Formulation
Product Description
LOCTITE® LB 8009® Heavy Duty Anti-Seize is a premium graphite and calcium fluoride based anti-seize lubricant formulated to protect threaded assemblies and metal components exposed to extreme temperatures and harsh industrial environments. The metal-free formulation contains no lead, copper, sulfur, or related compounds, making it compatible with stainless steel and nickel alloys. It provides long-term lubrication, prevents galling and seizure, and facilitates disassembly of components operating from -29°C to +1315°C.
Key Features & Benefits
- Graphite and calcium fluoride anti-seize formulation.
- Free from lead, copper, sulfur and free metals.
- Compatible with stainless steel and nickel alloys.
- Protects against galling, seizing and corrosion.
- Provides improved clamp load consistency.
- Suitable for extremely high temperature applications.
- Non-curing lubricant paste.
Recommended Applications
- Bolts, screws, studs and nuts.
- Pipe joints, plugs and bushings.
- Extrusion and forming dies.
- Heat exchangers and shear blades.
- Metal bending and mechanical packings.
- Chemical plants, refineries, power plants and steel mills.
- Marine, aerospace and industrial maintenance applications.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Condition |
|---|---|---|---|
| Technology | Anti-Seize Lubricant | — | Graphite / calcium fluoride formulation |
| Appearance | Grey Paste | — | Non-curing |
| Specific Gravity | 1.15 | — | 25°C |
| Penetration | 270 - 370 | 0.1 mm | ISO 2137 |
| Weight per Gallon | 9.6 - 10.6 | lb/gal | Typical |
| Metal Content | None | — | Lead, copper and sulfur free |
| Compatibility | Stainless Steel & Nickel Alloys | — | Suitable for corrosion-sensitive assemblies |
After-Processing / Final-State Properties
| Property | Value | Unit | Condition / Method |
|---|---|---|---|
| Operating Temperature Range | -29 to +1315 | °C | Continuous service range |
| Torque Coefficient (K Factor) | 0.16 | — | Lubricated 12.7 mm grade 8 steel bolt |
| Torque Coefficient (K Factor) | 0.27 | — | Unlubricated solvent-cleaned bolt |
| Clamp Load Efficiency | Improved | — | Provides higher clamp load at equivalent torque |
| Clamp Load Uniformity | Enhanced | — | More consistent bolt preload distribution |
| Corrosion Protection | Excellent | — | Protects threaded assemblies from seizure |
| Galling Resistance | Excellent | — | For stainless steel and alloy assemblies |
| Disassembly Protection | Prevents Seizing | — | Facilitates future maintenance |