LOCTITE LB8036
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

Main features
- Non-Metallic Grease Material
- High-Lubricity Thread Assembly
- 29C to 1093C Service Temperature
Product Description
LOCTITE® LB 8036 White High Temperature Anti-Seize is a premium non-metallic anti-seize compound designed to prevent galling, seizing, and corrosion of threaded and mated metal components exposed to extreme temperatures and harsh environments. The aluminum complex based formulation provides excellent lubricity, superior water resistance, and protection against galvanic corrosion while allowing easier assembly and disassembly of components. The product is compatible with a wide variety of metals including copper, brass, cast iron, steel, stainless steel, and other alloys.
Key Features & Benefits
- Non-metallic anti-seize formulation.
- Typical service temperature range from -29°C to 1093°C.
- Excellent lubricity for threaded assemblies.
- Superior water washout resistance.
- Superior water spray resistance.
- Prevents galvanic corrosion.
- Permits easy assembly and disassembly of metal parts.
Recommended Applications
- Bolts, screws, studs and nuts.
- Pipe joints, shafts and bushings.
- Splines, chains and cables.
- Crane assemblies and industrial ovens.
- Power plant turbine studs and inlet heater assemblies.
- Coal crushers, pulp and paper mills.
- Water and wastewater treatment facilities.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-Supplied / Before-Processing Properties
| Property | Value | Unit | Condition |
|---|---|---|---|
| Technology | Anti-Seize Compound | — | Non-metallic formulation |
| Chemical Type | Aluminum Complex | — | Base thickener system |
| Appearance | White Paste | — | As supplied |
| Specific Gravity | 1.10 | — | Typical value |
| Unworked Penetration | 320 | mm/10 | ASTM D217 |
| Worked Penetration (60 strokes) | 322 | mm/10 | ASTM D217 |
| Flash Point | >200 | °F | TCC |
| Weight per Gallon | 9.2 | lb/gal | Typical value |
After-Processing / Final-State Properties
| Property | Value | Unit | Condition / Method |
|---|---|---|---|
| Service Temperature Range | -29 to +1093 | °C | Typical operating range |
| Lubricity K-Factor | 0.164 | — | 5,000 lb clamp load |
| Lubricity K-Factor | 0.166 | — | 6,000 lb clamp load |
| Water Washout | 0.33 | % | ASTM D1264 |
| Copper Corrosion | No Visible Change | — | ASTM D130-94 |
| Oil Separation | 0.94 | % | FTM 791 Method 321.3 |
| Salt Fog Corrosion Resistance | No Visible Change | — | ASTM B117 |
| Galvanic Corrosion Protection | Excellent | — | Multi-metal assemblies |
| Water Spray Resistance | Superior | — | Wet environments |