LOCTITE SF7090

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE SF7090

Main features

  • Accelerates Cure of Loctite Anaerobic Adhesives
  • Solvent-Free Bonding Formulation
  • Passive Metals and Inert Materials

Product Description

LOCTITE® SF 7090™ is a reactive monomer-based, solvent-free surface activator designed to accelerate the cure speed of LOCTITE® anaerobic adhesives and sealants. It is particularly effective for use on passive metals, inert surfaces, large bond gaps, and low-temperature applications below 15°C. The activator promotes rapid fixture and cure development while remaining active on treated surfaces for up to one hour after application.

Key Features & Benefits

  • Accelerates cure of LOCTITE® anaerobic adhesives and sealants.
  • Solvent-free reactive monomer formulation.
  • Ideal for passive metals and inert substrates.
  • Improves curing across large bond gaps.
  • Recommended for low-temperature applications (<15°C).
  • Can be applied by spray or brush.
  • Remains active on surfaces for up to one hour.

Recommended Applications

  • Acceleration of anaerobic threadlockers.
  • Acceleration of anaerobic retaining compounds.
  • Passive metal assemblies.
  • Large bond gap assemblies.
  • Low-temperature bonding operations.
Product Family

LOCTITE SF7090

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Dark blue-green liquid
Specific GravitySpecific Gravity
1.03
Physical Properties
ViscosityViscosity
10 - 25 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Activator For anaerobic adhesives and sealants
Chemical Type Copper Salt and Aliphatic Amine Reactive activator chemistry
Solvent Reactive Methacrylate Monomer Solvent-free system
Appearance Dark Blue-Green Liquid As supplied
Specific Gravity 1.03 25°C
Viscosity 10 - 25 mPa·s (cP) Brookfield RVT, 25°C
Part Life ≤1 hour Activated surface life
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Fixture Time ≤25 seconds Steel, ISO 4587, LOCTITE® 326™, two-side activation
Activator Open Time Up to 1 hour Activator remains effective after application
Application Method Spray or Brush Apply to mating surfaces
Large Gap Performance Enhanced Promotes cure in larger bond gaps
Passive Metal Performance Enhanced Improves cure on passive substrates
Low Temperature Suitability Recommended Below 15°C operating conditions
Cure Acceleration Function High For LOCTITE anaerobic products

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers