LOCTITE TCP 7000 Printable Phase-Change Thermal Interface Material is a gray, non-silicone phase-change thermal interface paste formulated for stencil or screen printing between heat-generating devices and heat-dissipating surfaces. The cartridge-supplied material dries to a solid layer, then flows at its 45 deg C phase-change temperature to conform at the interface. Dried material has thermal conductivity greater than 3.0 W/(m K) by ASTM D5470 and an operating range up to 150 deg C. It is reworkable and is formulated to avoid pump-out, dry-out, and silicone migration in processors, memory devices, power modules, IGBTs, and active heat-sink assemblies.

Key features

  • Stencil and Screen Printing: Supports patterned application through stencil or screen processes.
  • Reworkable Silicone-Free Interface: Provides a removable interface without silicone migration.
  • 45 deg C Phase Change: The dried layer flows at the phase-change temperature to conform at the interface.

Applications

Applications include microprocessors, GPUs, multi-chip modules, ASICs, IGBTs, FBDIMMs and other memory devices, lidded processors, active heat sinks, power modules, and high-power electronics.

Product Family

LOCTITE TCP7000

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Operating TemperatureOperating Temperature
up to 150 °C
Thermal ConductivityThermal Conductivity
>3.0 W/m.K
General Properties
Component SystemComponent System
Phase Change Material
Specific GravitySpecific Gravity
2

Additional Information

Technical properties

As-supplied paste properties

Property Value Unit Method / condition
Appearance Gray paste As supplied
Specific gravity 2.0 g/cm^3 As supplied
Application method Stencil or screen printing Inline dispensing is not recommended
Maximum recommended thickness 254 um For complete drying under normal conditions
Storage life 365 days Stored at 2 to 8 deg C
Technical properties

Dried interface properties

Values apply after the printed material has been dried using an appropriate thickness-dependent schedule.

Property Value Unit Method / condition
Phase-change temperature 45 deg C DSC
Thermal conductivity >3.0 W/(m K) ASTM D5470, dried material
Operating temperature Up to 150 deg C Dried interface

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers