MOLYKOTE G684OZTUBES
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

Main features
- Plastic Gear Friction Control
- 75 mm2/s Base Oil
- Brush-to-Central System Application
Product Description
MOLYKOTE G-68 Plastic Gear Grease, 4 oz Tube is a 4 oz tube configuration of the mineral-oil/PAO G-68 plastic gear grease grade. The grease uses lithium soap, EP additives, and solid lubricants and has NLGI 2-3 consistency, 75 mm2/s base-oil viscosity at 40 deg C, and a -30 to 140 deg C service range. It can be applied by brush, spatula, grease gun, automatic device, or central lubrication system. Applications include electric toothbrush and paper-shredder gears and related plastic gear mechanisms using the G-68 grade.
Key features
- Plastic Gear Friction Control: The G-68 grade produced a 0.014 steel-ball/POM friction coefficient under the specified test conditions.
- 75 mm2/s Base Oil: The G-68 grade has 75 mm2/s base-oil viscosity at 40 deg C.
- Flexible Grease Application: Supported methods include brush, spatula, grease gun, automatic device, and central lubrication system.
Applications / Suitable for
- Gears in electric toothbrushes.
- Gears in paper shredders.
- Plastic gear mechanisms using the G-68 grade.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied grease properties
Technical values apply to the MOLYKOTE G-68 grease grade.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| NLGI consistency class | 2-3 | DIN 51818; G-68 grade, typical | |
| Worked penetration | 250 to 280 | mm/10 | ISO 2137; G-68 grade, typical |
| Density | 0.85 | g/ml | ISO 2811 at 20 deg C; G-68 grade, typical |
| Base-oil viscosity | 75 | mm2/s | DIN 51562 at 40 deg C; G-68 grade, typical |
| Drop point | 190 | deg C | ISO 2176; G-68 grade, test result |
In-service performance properties
Technical values apply to the MOLYKOTE G-68 grease grade.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Service-temperature range | -30 to 140 | deg C | G-68 grade, typical |
| Four-ball weld load | 1,900 | N | DIN 51350, Part 4; G-68 grade, typical |
| Four-ball wear scar | 0.75 | mm | DIN 51350, Part 5 under 600 N load; G-68 grade, typical |
| Almen-Wieland OK load | 18,500 | N | G-68 grade, typical |
| Steel/POM friction coefficient | 0.014 | 12.7 mm steel ball, 6.3 N, 10 mm/s, 24 h; G-68 grade, typical | |
| Oil separation | 3.4 | % | DIN 51817 / Federal Standard 791-32-2; G-68 grade, typical |