OPTOLINQ BMC-4200| Opaque Mold Compound
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- Opaque
- Suitable spiral flow for molding conditions
- Superior reliability
Product Description
OPTOLINQ BMC-4200 is a Series of Opaque molding compounds used as encapsultation of optoelectronic devices. It exhibits excellent moldability under suitable spiral flow conditions.
This material exhibits excellent thermal stability, meaning it can withstand high temperatures without significant degradation. Additionally, it possesses outstanding mechanical processing performance, making it easily moldable and shapeable during manufacturing.
The material's remarkable moldability allows for precise and intricate molding of optoelectronic devices, ensuring consistent and high-quality production. Furthermore, its superior reliability ensures that the molded devices maintain their performance and functionality over extended periods, making it a highly dependable choice for optoelectronic applications.
Molding information
OPTOLINQ BMC-4200 differs from other molding compounds and has some special procedures required.
Temperature recovery
OPTOLINQ BMC-4200 must first be allowed to achieve room temperature (20±5°C , 40±15% RH) for atleast 24 hours (Big size) and 12 hours (Small size), without opening the bag before using it, to avoid contamination.
Preheat
Preheating of OPTOLINQ BMC-4200 can be done by using standard RF equipment. The preheating should be done slowly to achieve uniform temperature.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Curing Conditions
Additional Information
Featured BMC-4200H Variants: KRAYDEN Product Offerings

OPTOLINQ BMC for Filter Applications
Looking to enhance optical precision and durability in your filter-integrated optoelectronic devices? This short presentation introduces OPTOLINQ’s optical molding compounds specifically designed for high-performance filter applications.
Featuring BMC-4200H, a versatile formulation available in six onset wavelengths (700, 720, 750, 820, 840, and 870 nm), our optical compounds offer exceptional light control, environmental resistance, and long-term optical clarity.
Whether you're fine-tuning signal filtering, improving IR sensitivity, or ensuring high transmission and structural stability, OPTOLINQ compounds are built to perform—consistent, and reliable.
Got questions or need help selecting the right optical grade for your filter applications? Reach out to us!
Contact Us →