Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- High-Viscosity Non-Drip Threadlocking
- MIL-S-46163A/MIL-S-22473E/ASTM D5363 Compliance
- Vibration/Corrosion-Resistant Thread Retention
Product Description
Permabond® HH120 is an excellent general-purpose anaerobic threadlocker and sealant designed for the permanent assembly of bolts, nuts, and screws. Featuring a high-viscosity, non-drip, and thixotropic formulation, it is particularly well-suited for coarse threaded fasteners where precise application without slumping is required. It cures fast and reliably at room temperature on various metal surfaces, including steel, cadmium, zinc, and other plated fasteners, providing exceptional environmental and corrosion resistance.
Key features
- Military and Industry specified: Tested to meet the strict requirements of MIL-S-46163A, MIL-S-22473E, and ASTM D5363 standards.
- High viscosity & Non-drip: The 7,000 cP thixotropic formulation ensures the adhesive stays in place, making it ideal for coarse threads and blind holes.
- Vibration and corrosion protection: Reliably prevents vibration loosening while providing a 100% solid, environmentally friendly barrier against corrosion.
Applications / Suitable for
- Permanent locking of coarse threaded fasteners, bolts, nuts, and screws
- Sealing pipe flanges and retaining worn bearings
- Machinery and equipment manufacturing
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Electrical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Composition | Methacrylate esters | - | - |
| Appearance | Red | - | Liquid |
| Viscosity | ~ 7,000 | cP / mPa.s | at 25°C |
| Specific Gravity | 1.1 | - | - |
| Maximum Gap Fill | 0.25 | mm | (0.01 in) |
| Maximum Thread Size | M30 | - | (1 1/4") |
| UV Fluorescence | Yes | - | - |
| Flash Point | > 100 | °C | - |
| Volatile Organic Compound | < 2 | % | 20 grams/liter (Estimated) |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Handling Strength Time | 10 | minutes | M10 steel at 23°C |
| Working Strength Time | 30 | minutes | M10 steel at 23°C |
| Full Strength Time | 24 | hours | M10 steel at 23°C |
| Breakaway Torque Strength | 31 | N-m | M10 steel (ISO 10964) (275 in.lb) |
| Prevailing Torque Strength | 34 | N-m | M10 steel (ISO 10964) (300 in.lb) |
| Shear Strength | 17 | MPa | Steel collar & pin (ISO 10123) (2500 psi) |
| Coefficient of Thermal Expansion | 90E-6 | mm/m/°C | - |
| Dielectric Strength | 11 | kV/mm | - |