HB3 | Quartz Sand 99.97%
Harmonization Code : |

Main features
- ≥99.97% SiO2
- High purity
- Flexible Particle Size
Product Description
HB3 Quartz sand Silica is produced from chemically treated and water washed high purity quartz. The milling process ensures minimal contamination, resulting in high purity silica sand of up to a SiO2 content of 99.97%.
HB3 Quartz sand Silica is an inherently inert white product, with low moisture, commonly used in the outer lining of crucibles and quartzware. The silica sand is tested and controlled to rigorous standards which ensure consistent chemical and physical properties resulting in predictable and repeatable performance.
TDS, SDS & Technical Documents
Technical Specifications
Chemical Properties
Silicon Dioxide(SiO2)Silicon Dioxide(SiO2)
99.97 %Additional Information
Particle Size Analysis
| Microns | % Finer |
| 250 | 99.5 |
| 200 | 75 |
| 180 | 50 |
| 125 | 20 |
| 100 | 3 |
Typical Values. They do Not Represent A Specification