HB4 | Quartz Sand 99.99%
Harmonization Code : |

Main features
- ≥99.99% SiO2
- Very High purity
- Flexible Particle Size
Product Description
HB4 Quartz sand Silica is our medium range Quartz sand. It has very low alpha ray emissions, very low iron, chromium, copper and Manganium and a SiO2 content of 99.99%.
HB4 Quartz sand Silica is an inherently inert white product, with low moisture that can be used for optical glass applications and fiber optic cable clading. It is tested and controlled to rigorous standards which ensure consistent chemical and physical properties resulting in predictable and repeatable performance. Particle size distribution is flexible and adjusted to the customer's needs.
TDS, SDS & Technical Documents
Technical Specifications
Chemical Properties
Silicon Dioxide(SiO2)Silicon Dioxide(SiO2)
99.99 %Additional Information
Particle Size Analysis
| Microns | % Finer |
| 250 | 99.5 |
| 200 | 75 |
| 180 | 50 |
| 125 | 20 |
| 100 | 3 |
Typical Values. They do Not Represent A Specification