ROYAL DOUBLE BUBBLE 04022
Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

Main features
- Fast One-Hour Handling Strength
- High-Peel Semi-Rigid Bonding
- Thermoplastic and Laminate Repair
Product Description
Hardman Double/Bubble 04022 Urethane D-50 Adhesive uses a 3.5 g premeasured, two-part polyurethane packet for fast structural bonding and repair. The beige mixed adhesive has a viscosity of 10,000 cP at 25 deg C, a 3 to 5 minute work time, and a 60 minute handling point. Its semi-rigid cured profile combines 65 Shore D hardness with typical 62 pli T-peel strength and 2,960 psi lap shear strength on acid-etched aluminum at 25 deg C. The maximum service temperature is 79 deg C. D-50 is used for engineering thermoplastics, SMC, laminated surfaces, automotive repairs, conveyor belts, and sporting-goods repair.
Key features
- Semi-rigid polyurethane bond: The cured adhesive combines peel, shear, impact, and fatigue resistance.
- Fast one-hour handling: A 3 to 5 minute work time is followed by 60 minute handling strength.
- High peel strength: Typical T-peel strength is 62 pli on acid-etched aluminum at 25 deg C.
Applications
Applications include bonding engineering thermoplastics, SMC, laminated surfaces, automotive components, conveyor belts, sporting goods, and other supported metal, plastic, or composite repairs.
TDS, SDS & Technical Documents
Technical Specifications
Thermal Properties
Additional Information
As supplied / before processing
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Package size | 3.5 | g | Premeasured dual-pouch packet |
| Part A viscosity | 13,000 | cP | At 25 deg C |
| Part B viscosity | 7,000 | cP | At 25 deg C |
| Mixed viscosity | 10,000 | cP | At 25 deg C |
| Mixed specific gravity | 1.27 | - | At 25 deg C |
| Work time | 3-5 | min | At room temperature |
| Handling strength | 60 | min | At room temperature |
| Shelf life | 12 | months | Part A and Part B |
After processing / final state
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 65 | Shore D | Tested at 25 deg C |
| Maximum service temperature | 79 | deg C | Cured adhesive |
| Lap shear strength | 2,960 | psi | Acid-etched aluminum-to-aluminum; tested at 25 deg C |
| Lap shear strength | 4,580 | psi | Acid-etched aluminum-to-aluminum; tested at -40 deg C |
| T-peel strength | 62 | pli | Acid-etched aluminum-to-aluminum; tested at 25 deg C |
| T-peel strength | 2.5 | pli | Acid-etched aluminum-to-aluminum; tested at 82 deg C |