ROYAL M6325
Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

Main features
- One-part paste application
- 15 to 45 minute tack-free
- Resilient elastomeric bond
Product Description
Royal Silaprene M6325 Adhesive/Sealant is a one-part gray polychloroprene adhesive/sealant supplied in a paste extrusion grade for room-temperature application. The material develops a tack-free surface in 15 to 45 minutes under ambient conditions and reaches an initial set in about four hours. It can be applied with a caulking gun or suitable pressure-pumping equipment and does not require component mixing, priming, or heating. After solvent evaporation, the elastomeric material forms a resilient bond and seal that continues to build strength over time.
Key features
- One-part paste: Applies without component mixing, priming, or heating
- Fast surface set: Tack-free in 15 to 45 minutes under ambient conditions
- Resilient elastomer: Forms a flexible bond and seal after solvent evaporation
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Chemistry TypeChemistry Type
PolychloropreneSolidsSolids
50 %Specific GravitySpecific Gravity
1.1Thermal Properties
Operating TemperatureOperating Temperature
-51 to 121 °C