Product Description

HT11000 is the product with the highest thermal conductivity in our entire product line. It is a Silicone based one-part Gap Filler provides a thermal conductivity of 11.0 W/m·K along with high compressibility. It is formulated to deliver high dispense rates for improved productivity, long-term reliability performance and to be easily reworkable.

HT11000 maintains excellent performance through reliability testing, and provide scalable applications at a competitive cost.  Additionally it performs great in oil,crack and slump testing and it exhibits no pump out and cracking risk.

You probably noticed the lack of information and specific product properties such as BLT, dispense rate and Thermal impedance. Since those are top of the line products, we go to certain extends to protect Honeywell's IP and competitive advantages. This generic flavor text cannot really describe how good this product is. A plethora of information,  including additional data,  images and samples are available once an NDA is in place. Contact us for more details.

 

Product Family

SOLSTICE HT11000

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Dark Gray
Thermal Properties
Thermal ConductivityThermal Conductivity
11 W/m.K

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers