LOCTITE STYCAST A316-48

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE STYCAST A316-48

Main features

  • Non conductive
  • High Tg
  • Fast cure

Product Description

LOCTITE STYCAST A316-48 is an oxide filled, pourable epoxy adhesive designed for use in harsh automotive applications. It is a one component, heat resistant epoxy with exceptional thermal stability and chemical resistance.

LOCTITE STYCAST A316-48 cures in a few minutes in moderate temperatures and can adhere well on plastics, phenolics, metals and ceramics for heat resistant sensors and control modules. It is an automotive grade potting material with High glass transition temperature.

 

Cure Schedule

  • 30 minutes @ 100°C or
  • 5 minutes @ 120°C or
  • 3 minutes @ 140°C or
  • 1 minutes @ 160°C

Post Cure

  • 2 to 4 hours at the highest expected use temperature
Product Family

STYCAST A316-48

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 20 days
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.4
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
145 °C
Thermal ConductivityThermal Conductivity
0.4 W/m.K
Electrical Properties
Volume ResistivityVolume Resistivity
1000000000000000 Ohms⋅cm
Physical Properties
ViscosityViscosity
50,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers