TML - Total Mass Loss
% of a materials mass that evaporates when exposed to a vacuum and high temperature.
CVCM - Collected Volatile Condensible Material
The fraction of mass that evaporates from the material then condenses on a cold surface.
WVR - Water Vapor Recovered
% of water vapor released by the material under the same conditions that can condense on a a collector.
LINQTAPE™ PIT1A-LO is an amber high-temperature resistant polyimide film designed for both permanent and temporary bonding in many high-temperature applications.
| Product | Total Mass Loss (TML-WVR) | Condensed Volatiles (CVCM) | |
|---|---|---|---|
| PIT1A-LO | <1.0 % | <0.1 % | |
|
ASTM E 595 Standard |
<1.0 % | <0.1 % |
⚡ Applications
- Electrical Insulation
- Edge protection
- Vibration damping
- Thermal Stability
- Temporary or permanent masking
✅ Advantages
✔ Low outgassing
✔ Excellent high temperature resistance
✔ Electrical Insulation
Frequently Asked Questions about Low Outgassing Tapes
Low-outgassing tapes are used to protect sensitive components in environments where contamination from volatile compounds must be minimized. Common applications include aerospace, satellites, high-altitude aircraft, solar panels, and precision electronics. They provide electrical insulation, mechanical protection, and chemical stability without releasing gases that could compromise performance.
What specifications do I need to review when selecting a polyimide tape for an aerospace application?Aerospace outgassing tapes should have TML <1%, CVCM <0.1%, high temperature resistance (typically -70°C to 260°C), and strong adhesion without leaving residue.
These tapes typically use high-purity polyimide (Kapton) films combined with specialized low-volatility adhesives. Both components are processed and cured to remove residual solvents and ensure long-term chemical stability.
What would happen if I used a non-outgassing tape in an aircraft solar panel?Non- outgassing tapes can release volatiles that condense on cells, reducing efficiency and damaging contacts, while low outgassing tapes ensure long-term performance.
Introduction to Specialty Tapes
This presentation introduces the main types of specialty tapes and films, focusing on high-performance materials engineered for demanding environments. It explores adhesion properties, common tape constructions, typical applications across multiple industries, and best practices for selecting and using specialty tapes to achieve optimal performance and long-term reliability.
Materials for Specialty Tapes and Films
Curious about how the right materials can improve performance? This presentation showcases KRAYDEN's portfolio of specialty tapes and films, highlighting key material technologies, performance characteristics, and recommended applications. Learn how these solutions provide reliable bonding, insulation, protection, thermal management, and electrical performance across a wide range of electronics and industrial applications.
Related Blogs
Hydrogen Safety with Hydrogen Detection Tapes?
This blog explains how KRAYDEN’s hydrogen‑detection tapes help improve safety when working with hydrogen — a gas that’s highly flammable, diffuses quickly, and is very hard to detect because it’s colorless, odorless, and lighter than air.
Copper Foil Tape for EMI Shielding?
This blog discusses how copper foil tape is used for EMI (electromagnetic interference) shielding, static dissipation, and grounding in electronic devices. It highlights the tape’s conductive adhesive, easy application, and ability to protect sensitive circuits while improving signal integrity and device reliability.