CHEMLOK 6411
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

Main features
- 30-Minute Room-Temperature Dry
- 12.7 to 25.4 um Film
- Brush, Roll, Dip or Spray
Product Description
Chemlok 6411 Adhesive is a one-part, solvent-based, heat-reactive covercoat adhesive for bonding supported rubber compounds to metal and other rigid substrates. For general use, it is applied over Chemlok 205 or 207 primer, although selected systems may use it as a one-coat adhesive. Chemlok 6411 can be applied by brush, roll coat, dip, or spray and is used at a dry film thickness of 12.7 to 25.4 um. The applied film typically dries in about 30 minutes at room temperature, with hot-air drying available at temperatures up to 90 deg C.
Key features
- Primer-System Flexibility: normally used over Chemlok 205 or 207 primer, with selected one-coat applications also supported
- Multi-Method Application: applies by brush, roll coat, dip, or spray
- Room-Temperature Drying: applied film typically dries in approximately 30 minutes at room temperature
Applications
Bonding supported rubber compounds to metal and other rigid substrates, normally with the specified Chemlok primer system.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Black liquid | Typical | |
| Viscosity | 200 to 600 | cps | 25 deg C; Brookfield LVT, spindle 2, 30 rpm; typical |
| Density | 970 to 1010 | kg/m^3 | Typical |
| Solids by weight | 22 to 26 | % | Typical |
| Flash point | 25 | deg C | Seta; typical |
| Shelf life | 1 | year | Below 25 deg C; original unopened container |