DOWSIL Q2-1346

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

DOWSIL Q2-1346

Main features

  • Low Sodium and Potassium Impurity Limits
  • Clear Liquid Supplied Free from Suspended Matter
  • Long 900-Day Shelf Life

Product Description

DOWSIL™ Q2-1346 Diluent is a silicone diluent supplied as a clear liquid for use in compatible silicone formulations. The product is manufactured to a controlled sales specification with requirements for appearance and low extractable sodium and potassium levels. It offers a long shelf life when stored in its original unopened container under the specified storage conditions.

Key Features

  • Clear liquid free from suspended matter.
  • Controlled maximum sodium content of 2.00 ppm (extracted water).
  • Controlled maximum potassium content of 2.00 ppm.
  • Long shelf life of 900 days in the original unopened container.

Suitable For

  • Use in compatible DOWSIL™ silicone formulations.
Product Family

DOWSIL Q2-1346

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Clear Liquid

Additional Information

As-Supplied / Before-Processing Properties

Property Value
Appearance Clear liquid, free from suspended matter
Sodium (in extracted water) 2.00 ppm maximum
Potassium 2.00 ppm maximum
Shelf Life 900 days
Storage Conditions No specific storage requirements; store in original unopened container

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers