KRAYDEN is proud to offer its own LINQTAPE™ PET-Series brand of high-performance, flexible, polyester film with Silicone and Acrylic adhesives for a range of applications.
High Performance Polyester Tape and Film
Polyester is a less-expensive material, but is limited to applications that have a maximum of 200°C. Therefore, it is preferred over Polyimide for applications up to 200°C. These applications include but are not limited to masking, temporary bonding, and splicing in industries that range from semiconductor, to automotive to general manufacturing. For applications that see temperatures up to 260°C, then you should use polyimide tapes and films.
LINQTAPE™ PET-Series films and tapes typically come in 33 meter (36 yard) length rolls of varying widths. and the base polyester film (backing) thickness range is between 1-mil (25µm) and 5-mil (125µm) thick. Other widths, lengths and thicknesses may be available upon request.